Synthesis and Oxidation Behavior of Platinum-Enriched γ+γ’ Bond Coatings on Ni-Based Superalloys

By:
Zhang, Ying; Ballard, D; Stacy, J; Pint, Bruce A; Haynes, James A
Journal Name:
Surface and Coatings Technology
Page Number:
3857-3861
Volume:
201
Issue Number:
7
Publication Date:
January 2007