Relationship between Yield Point Phenomena and the Nanoindentation Pop-in Behavior of Steel

By:
Ahn, T.-H.; Oh, C.-S.; Lee, K.; George, Easo P; Han, H.
Journal Name:
Journal of Materials Research
Page Number:
39-44
Volume:
27
Issue Number:
1
Publication Date:
January 2012
View DOI Listing:
https://doi.org/10.1557/jmr.2011.208