July 2017

Journal

Indentation Schmid factor and incipient plasticity by nanoindentation pop-in tests in hexagonal close-packed single crystals Last checked 5-30-17

By:
Zhang, Wei ; Gao, Yanfei ; Xia, Yuzhi; Bei, Hongbin
Journal Name:
Acta Materialia
Page Number:
53-65
Volume:
134
Issue Number:
N/A
Publication Date:
July 2017
View DOI Listing:
https://doi.org/10.1016/j.actamat.2017.05.058