Dislocation decorrelation and relationship to deformation microtwins during creep of a γ′ precipitate strengthened Ni-based superalloy

By:
Unocic, Raymond R; Zhou, Ning; Kovarik, Libor; Shen, Chen; Wang, Yunzhi; Mills, Michael
Journal Name:
Acta Materialia
Page Number:
7325-7339
Volume:
59
Issue Number:
19
Publication Date:
September 26, 2011
View DOI Listing:
https://doi.org/10.1016/j.actamat.2011.07.069

Abstract

The evolution of microtwins during high temperature creep deformation in a γ′ strengthened Ni-base superalloy has been investigated through a combination of creep testing, transmission electron microscopy (TEM), theoretical modeling, and computer simulation. Experimentally, microtwin nucleation sources were identified and their evolution was tracked by characterizing the deformation substructure at different stages of creep deformation. Deformation is highly localized around stress concentrators such as carbides, borides and serrated grain boundaries, which act as sources of a/2 matrix-type dislocations. Due to fine channels between γ′ particles, coupled with the low γ matrix stacking fault energy, the a/2 matrix dislocations dissociate into a/6 Shockley partials, which were commonly observed to be decorrelated from one another, creating extended intrinsic stacking faults in the γ matrix. Microtwins are common and form via Shockley partial dislocations cooperatively shearing both γ and γ′ phases on adjacent {111} glide planes. The TEM observations lead directly to an analysis of dislocation-precipitate interactions. Through phase field simulations and theoretical analyses based on Orowan looping, the important processes of dislocation dissociation and decorrelation are modeled in detail, providing comprehensive insight into the microstructural features and applied stress conditions that favor the microtwinning deformation mode in γ′ strengthened Ni-based superalloys.