November 2020

Journal

Roll-To-Roll Atomic Layer Deposition of Titania Nanocoating on Thermally Stabilizing Lithium Nickel Cobalt Manganese Oxide Cathodes for Lithium Ion Batteries

By:
Hsieh, Chien-Te; Chao, Chia-Hung; Ke, Wen-Jie; Lin, Yeou-Fu; Liu, Hao-Wei; Gandomi, Yasser; Gu, Siyong; Su, Cherng-Yuh; Chang, Jeng-Kuei; Li, Jianlin ; Fu, Chun-Chieh; Mallick, Bikash; Juang, Ruey-Shin
Journal Name:
ACS Applied Energy Materials
Page Number:
10619-10631
Volume:
3
Issue Number:
11
Publication Date:
November 2020
View DOI Listing:
https://doi.org/10.1021/acsaem.0c01541

Abstract

Conformal coating of ceramic layers (nm-thick) on Ni-rich layered cathode materials is an effective strategy for improving high-temperature longevity of Li-ion batteries (LIBs). In this work, we develop a roll-to-roll atomic layer deposition (R2R ALD) apparatus for growing uniform nanolayers of TiO2. We explore the effect of ALD parameters (temperature: 120–180 °C and line speed: 2–40 mm s–1) on the TiO2 surface coating and subsequently investigate the electrochemical performance of the as-prepared cathodes. The capacity retention of TiO2-coated porous electrodes is substantially improved compared to that of the pristine cathode material for high-temperature cycling. Electrochemical impedance spectroscopy confirms that the ALD-TiO2 coating suppresses the undesired side reactions initiated at the electrode/electrolyte interface, reduces charge transfer resistance, and ultimately facilitates the Li+ transport through the composite cathode nanostructure. The robust design of the ALD-TiO2 cathode material enables high-temperature operation (>55 °C) with enhanced specific capacity, superior rate capability, excellent cyclability, and ultra-high coulombic efficiency within a wide potential window (3.0–4.35 V). The R2R ALD technique developed in this work paves the way for large-scale fabrication of ceramic-coated cathode sheets with a production rate reaching 2.4 m min–1 for a continuous coating operation.