Nanoindentation Mechanical Properties Characterization of Glassy Polymeric Carbon Treated with Ion Beam

By:
Rodrigues, M.; Da Cruz, N.; Rangel, E.; Zimmerman, R.; Ila, Daryush; Poker, David B; Hensley, Dale K
Journal Name:
Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms