ORNL Report

High-Temperature Tensile and Creep Test Results on Thin Wall Tube Specimens of ODS Alloys 14YWT and OFRAC

By:
Hoelzer, David T; Stinson, Ian A; Massey, Caleb P
Publication Date:
June 2022