August 2009

Journal

Edge-Localized-Mode Suppression through Density-Profile Modification with Lithium-Wall Coatings in the National Spherical Torus Experiment

By:
Maingi, Rajesh ; Osborne, T.; LeBlanc, B; Bell, R. E.; Manickam, J.; Snyder, P.; Menard, J.; Mansfield, D.K.; Kugel, H.; Kaita, R.; Gerhardt, S.P.; Sabbagh, S. A.; Kelly, F.A.
Journal Name:
Physical Review Letters
Page Number:
075001
Volume:
103
Issue Number:
7
Publication Date:
August 2009
View DOI Listing:
https://doi.org/10.1103/PhysRevLett.103.075001

Abstract

Reduction or elimination of edge localized modes (ELMs) while maintaining high confinement is essential for future fusion devices, e.g., the ITER. An ELM-free regime was recently obtained in the National Spherical Torus Experiment, following lithium (Li) evaporation onto the plasma-facing components. Edge stability calculations indicate that the pre-Li discharges were unstable to low-n peeling or ballooning modes, while broader pressure profiles stabilized the post-Li discharges. Normalized energy confinement increased by 50% post Li, with no sign of ELMs up to the global stability limit.