October 2021

Journal

Construction of Inverse Metal–Zeolite Interfaces via Area-Selective Atomic Layer Deposition

By:
Zhai, Peng; Zhang, Laibao; Cullen, David A; Aireddy, Divakar; Ding, Kunlun
Journal Name:
ACS Applied Materials & Interfaces
Page Number:
51759-51766
Volume:
13
Issue Number:
43
Publication Date:
October 2021
View DOI Listing:
https://doi.org/10.1021/acsami.1c15569

Abstract

The spatial confinement at metal–zeolite interfaces offers a powerful knob to steer the selectivity of chemical reactions on metal catalysts. However, encapsulating metal catalysts into small-pore zeolites remains a challenging task. Here, we demonstrate an inverse design of metal–zeolite interfaces, “metal-on-zeolite,” constructed by area-selective atomic layer deposition. This inverse design bypasses the intrinsic synthetic issues associated with metal encapsulation, offering a potential solution for the fabrication of task-specific metal–zeolite interfaces for desired catalytic applications. Infrared spectroscopy and several probe reactions confirmed the spatial confinement effects at the inverse metal–zeolite interfaces.


Related Researchers