September 2009

Conference Paper

Chemical and Mechanical Analysis of HDIS Residues using Auger Electron Spectroscopy and Nanoindentation

By:
Kadavanich, Andreas V; Shim, Sang Hoon ; Meyer III, Harry M; Savas, Stephen; Lara-Curzio, Edgar
Journal Name:
Solid State Phenomenon
Page Number:
261-264
Volume:
145
Issue Number:
N/A
Publication Date:
September 2009
Conference Name:
9th International Symposium on ULTRA CLEAN PROCESSING OF SEMICONDUCTOR SURFACES
Conference Location:
Brugge, Belgium

Abstract

Photoresist stripping after ion implantation at high dosages (>1E15 atoms/cm2) is the most challenging dry strip process for advanced logic devices. Such high-dose implant stripping (HDIS) frequently leaves residues on the wafers after dry strip, unless fluorine chemistries are employed in the stripping plasma. Silicon loss requirements at sub-45nm nodes generally preclude such aggressive stripping chemistries. Instead, a wet clean is used to remove residues. However, the nature of the residues is not well understood, and are believed to usually contain some of the cross-linked, carbonized organic polymer formed in the implant [1]. In this paper we present chemical and mechanical data on HDIS residues produced from oxidizing and reducing chemistry strip processes