An experimental evaluation of the constant beta relating the contact stiffness to the contact area in nanoindentation

By:
Strader, Jeremy; Shim, Sanghoon; Bei, Hongbin ; Oliver, Warren; Pharr, George M
Journal Name:
Philosophical Magazine A
Page Number:
5285-5298
Volume:
86
Issue Number:
33-35
Publication Date:
December 2006